HOW TO TEST EVA FILM SAFETY LAMINATED GLASS?

How to Test Eva Film Safety Laminated Glass

HOW TO TEST EVA FILM SAFETY LAMINATED GLASS?
BY PETER LIN

How to test Tensile Strength, Adhesive Strength of EVA Film laminated glass?

[Universal Testing Machine]
We can use this equipment to test the Tensile Strength of EVA Film, and also the Peeling Strength(equal to Adhesive Strength) between the EVA Film and Glass surface, or between the polymer sheet surface and EVA Film after heating(cross-linked).

How to test Impact Resistance of EVA Film laminated glass?

[Impact Testing Equipment]
You can use this to test the Impact Resistance of the laminated glass made of the EVA Film.

How to test Aging Resistance(equal to UV Radiation Resistance)?

[UV Radiation Accelerating Aging Tester]
Accelerated Aging Tester adopts fluorescent UV light UVA-340 and the water-spray system in order to imitate the damage of sunlight, rain, humidity etc.
The EVA laminated glass samples is under UV radiation damage and the water spray damage circularly.The damage intensity would be more than 10 times of the damage in the natural environment.
The damage is like: fading, changing color, delamination, haze, bubbles, embrittlement , aging, oxidation etc.

How to test Heat Resistance, Humidity Resistance and Weather Resistance of EVA Film laminated glass?

[Constant Temperature and Humidity Test]
You can test EVA Film laminated glass under great humidity environment or high temperature.
And you can also test EVA Film laminated glass under cold and hot circling environment, like -40degree C for 30 minutes and 85 degree C for 30 minutes as a circle

How to test the Haze of EVA Film laminated glass?

[Haze Tester]
You can test the haze of the laminated glass made of EVA Film, and also the transmittance of laminated glass made of EVA Film.

How to test Cross-link rate of EVA Film laminated glass after heating?

[Testing System for Gel Content Determination of Cross-link of Laminated EVA Film]
To see how many percent of gel content of the EVA Film after laminating heating (after cross link reacted). Which equals to how many percentage of EVA FILM is cross-linked.

How to test Transmission Values of UV(ultraviolet radiation), Visible Light and Infrared Ray of EVA FILM laminated glass in easy way?

[Laminated Glass Spectrometer]
It is able to simultaneously measure the Transmission Values of UV(ultraviolet radiation), Visible Light and Infrared Ray. The Spectrometer is self-contained light sources and automatic calibration. No man-driven adjustment is needed. The users only need to plug the power supply, turn on the switch and put the Laminated Glass in the opening. Then the measure data would appear on the display automatically.

How to UV Radiation Blacked Rate of EVA Film laminated glass?

[Spectrophotometer]:
Test the UV radiation blacked rate of laminated glass made of EVA Film. You can test the blacked rate at different wave-length.

If i need support to buy, build, install, use the test equipment, whom can i ask for help?

Please don’t hesitate to contact Peter Lin at [email protected] whenever you need support?

Peter Lin-CNCGLASS

SUPER CLEAR
SUPER CLEAR
WHITE
WHITE
COLOR
COLOR

Published by

[email protected] EVA film glass interlayer

Peter Lin Mail: [email protected] [email protected] Whatsapp: 0086 15013829504 Super clear eva film Outdoor white eva film series Green tape for laminating, heating resistant