Attentions for Manufacturing Different Kind of Pre-Laminated Glass
It’s better not to laminate different kind of Pre-laminated glass at the same time.
Because the time and temperature they need may be different.
Generally speaking:
(1) Colored EVA Film need higher temperature than clear EVA Film.
(2) Thicker EVA Film or thicker glasses need longer heating time.
(3) Sandwiched decorative interlayer like fabric need longer heating time than the simple no sandwiched laminated glass.
(4) Sometimes, you the decorative interlayer can not stand higher temperature, may be you can processing in lower temperature and prolong the heating time. But for the detail data, you should ask the EVA Film manufacturer.